Brand Name : UNICOMP

Model Number : UNZ-450

Certification : CE

Place of Origin : China

MOQ : 1Set

Price : can negotiate

Payment Terms : T/T, L/C

Supply Ability : 10 sets per month

Delivery Time : 30 days

Packaging Details : Wooden Case, Waterproof, Anti-collision

Name : X-ray Inspection Machine

Application : Aluminum Casting, Iron Casting, Auto Parts, Wheels, Metal Products, Refractory Materials

Tube Voltage : 450KV (160KV, 225KV, 320KV for option)

X-ray Leakage : < 2.5uSv/h

Weight : 17.5 T

Power Consumption : 10 kW

Contact Now

Casting defects heat sinks, hot tears, cold-flow, drag-marks, missing material and cracks NDT X-Ray Inspection

Application Fields of X Ray Machine UNZ-450

● Engineering components
● Small aluminum castings, iron castings
● Auto parts, metal products

Technical Parameters and Specifications of X Ray Machine UNZ-450

System Parameters
Dimensions 2766mm*2813mm*2598mm(L*W*H)
Equipment weight 17.5T
Power 10 kW
Maximum penetration (FE) 80 mm
Detection range Φ550*200mm
Load weight 30kg
Work environment 5-40° ≤80%HR
Power supply Three-phase five wire system AC380V
X-ray leakage dose rate ≤2.5μSv/h
X-ray Generator
Tube voltage 450KV (160KV, 225KV, 320KV for option)
Power 700W / 1500W
Focal size 0.5mm
Detector (FPD)
Image area 250mm×300mm
Pixel matrix 1792×2176
Pixel pitch 139μm
Frame rate 9fps(1×1) 30 fps(2×2)
Software Function
Image processing brightness and contrast adjustment; stacking frames, window width and level adjustment; image enhancement, filtering, sharpening, invert, relief and bubble measure;ove, zoom in, zoom out, display image scaling, display the current mouse coordinates and gray values
Image measurement distance, radius, polygon, angle measurement; arrows and text labels; save the image after processing
Motion control the speed adjustment of each moving axis; CNC programming; manual operation;
Additional function
● CNC programmable control, to save the detection time of the bulk of the workpiece
● C type arm five detection mechanism, no dead angle detection
● Servo stepper motor drive, stable operation
● Voltage regulator, isolation, filtering, grounding and other protective functions are complete
● Set aside industrial cloud interface, data and pictures in real time upload, with traceability and large data analysis(optional)

* Specifications are subject to change without notice, All trademarks are the property of the system maker.

X-Ray Images

Dimensions and Appearance


Product Tags:

Cold Flow NDT X Ray Equipment

      

450KV NDT X Ray Equipment

      

Hot Tears X Ray Inspection Equipment

      
Quality 10 KW NDT X Ray Equipment For Casting Defects Heat Sinks / Hot Tears / Cold Flow for sale

10 KW NDT X Ray Equipment For Casting Defects Heat Sinks / Hot Tears / Cold Flow Images

Inquiry Cart 0
Send your message to this supplier
 
*From:
*To: Unicomp Technology
*Subject:
*Message:
Characters Remaining: (0/3000)